Petroleum resin used in rubber mixing


Specification:

Grades/Properties

PR-C4090

PR-C4100

PR--C4100

Testing Methods

Appearance

Granule

Granule

Granule

Eyeballing

Softening Point οC

85 ?5

95 ?5

105 ?5

GB/T4507 (Ring &Ball)

Color Ga

≤4

≤ 5

≤ 5

ASTM D-1544

Acid Value (KOHmg/g)

≤1

≤1

≤1

GB2895

Bromine Value (gBr/100g)

≤25 

≤25 

≤25 

Melt Viscosity cps

Testing by user's demand

Testing by user's demand

Testing by user's demand

ASTM D-3236

Flash Point οC

≥240

≥240

≥240

GB261
GB3536

Use:
PR-C4090, PR-C4100, PR-C4110 petroleum resin are a kind of hydrocarbon resin widely used in tyre rubber mixing. It has good compatibility with natural rubber( NR), synthetic rubber, polyethylene, polypropylene, SIS, SEBS, EVA etc.. It is also used as tackifier,reinforcing agent,softener and filler etc.in rubber mixing.

Properties in rubber mixing:
?Excellent tackify property.
?Improve extensibility and spalling resistance.
?Cure time and the physical properties after sulfuration are not affected.
?Avoid adhesive capacity to processing machinery.
?Help filling material distribute evenly.
?Proper color.

Application field recommended: mixing of tyre rubber.

Other use :
?Other rubber products, such as tread, shoes heel, floor, belt etc..
?Light-colored rubber daily-use products.
?Light-colored one can be used in pressure sensitive adhesive.

 


::: Sitemap About Us   |  Products   |  Contact us   |  Order online   |  Chinese